MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 200B Polyethylene, Film Extrusion
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Bapolene 200B is is a general purpose low density polyethylene for blown film extrusion applications requiring superior clarity. This product meets US FDA 21 CFR 177.1520.

Applications: Film; Food Packaging; General Purpose; Industrial Applications; Packaging.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Food Contact Acceptable; High Clarity
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D-4883
Thickness 2.00 mil
Melt Flow 2.0 g/10 minASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 300 %ASTM D-882
Film Elongation at Break, TD 500 %ASTM D-882
Elmendorf Tear Strength MD 360 gASTM D-1922
Elmendorf Tear Strength TD 130 gASTM D-1922
Dart Drop Test 95.0 g
@Thickness 25.4 mm
ASTM D1709
Film Tensile Strength at Break, MD 24.1 MPaASTM D-882
Film Tensile Strength at Break, TD 18.6 MPaASTM D-882
1% Secant Modulus, MD 193 MPaASTM D-882
1% Secant Modulus, TD 214 MPaASTM D-882
 
Optical PropertiesOriginal ValueComments
Haze <= 8.0 %
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Bamberger Polymers Bapolene® 105F Low Density Polyethylene Film Resin
Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade
Overview of materials for Low Density Polyethylene (LDPE), Molded
Bamberger Polymers Bapolene® 107B Low Density Polyethylene Film Extrusion Resin

PBP3B380 / 20839

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.