MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 4142H Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Oil quenched. Forging temp.: 1205°C (2200°F) max. Annealing temp.: 790 - 845°C. Hardening temp.: 845 - 870°C. Tempered to desired hardness.

Medium hardenability. Applications include break dies, bending dies, support tooling, die holders, gears, flanges, collets, arbors, spindles, axles, clutch parts, forming rolls, wrenches and other hand tools, and various machine tool components.

Key Words: alloy steels, UNS H41420, ASTM A304, SAE J1268, DIN 1.7223
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 187 - 229
Hardness, Knoop 230Converted from Brinell
Hardness, Rockwell B 94Converted from Brinell
Hardness, Rockwell C 15Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 218Converted from Brinell
Modulus of Elasticity 206 GPaAISI 4142
Bulk Modulus 163 GPaEstimated from elastic modulus
Poissons Ratio 0.29Typical for steel
Machinability 65 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaEstimated from elastic modulus
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000263 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.473 J/g-°C
Thermal Conductivity 42.6 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.39 - 0.46 %
Chromium, Cr 0.75 - 1.2 %
Iron, Fe 96.615 - 97.91 %As remainder
Manganese, Mn 0.65 - 1.1 %
Molybdenum, Mo 0.15 - 0.25 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4142 Steel, Annealed and Cold Drawn
AISI 4142 Steel, Quenched and Tempered to 380 HB
AISI 4140 Steel, oil quenched, 100 mm (4 in.) round (845°C (1550°F) quench, 650°C (1200°F) temper)
AISI 4340 Steel, normalized, 100 mm (4 in.) round
AISI 4140H Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round

M4142B / 7555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.