MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polimix RF11/20 Polyester Bulk Moulding Compoud
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: BMC (Bulk Moulding Compoud) is a reinforced composite material that consists of the mixture of thermosetting resins; glass fiber; cut wire; fillers; additional components

Application of this grade: BMC can be used for both compression and injection molding. Injection use is particularly efficient when it comes to production of small technical parts in high quantities. In these cases the BMC loaded into the hopper of the injection molding machine enables high productivity through short cycle times and multi-cavity molds.

Production process: It is produced by mixing polyester resin and main additives and the paste is transferred to a kneading machine in which the chopped is added through a dosing system the chopped glass fiber (pre-cut), typically at 6 or 12 mm. After appropriate processing cycles with clockwise and counter-clockwise movements of the blades of the kneading machine the mixture obtained is forced through a transport screw into an outlet, with which the diameter of the packaging is determined. The cylinder obtained is placed in a styrene-impermeable bag and vacuum-sealed.

Application of this grade: Miniature circuit breaker

Information provided by Polmix SPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ISO 1183
Filler Content 20.0 %20.0 %Glass Fiber; ISO 1172
Water Absorption <= 0.100 %<= 0.100 %ISO 62
Linear Mold Shrinkage 0.00100 cm/cm0.00100 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 90.0 MPa13100 psiUNI EN ISO 178
Flexural Modulus 9.00 GPa1310 ksiUNI EN ISO 178
Charpy Impact, Notched 3.50 J/cm²16.7 ft-lb/in²UNI EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air >= 200 °C>= 392 °FHDT; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLM901 / 322933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.