MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Freudenberg Sealing Technologies 70 HNBR U463 Hydrogenated Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: HNBR is resistant to hot water and exhibits good cold and high temperature behavior. In sealing technology, the significantly more expensive HNBR, which is a proven standard material for automotive engine timing belts, is primarily used in applications where higher temperatures and/or mechanical strength are required. Its strength is above all in demand for rod and piston seals, along with O-rings, radial shaft seal rings, boots and diaphragms.

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc
@Temperature 23.0 °C
0.0405 lb/in³
@Temperature 73.4 °F
DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Temperature 23.0 °C
70
@Temperature 73.4 °F
DIN EN ISO 7619-1
Tensile Strength 19.0 MPa
@Temperature 23.0 °C
2760 psi
@Temperature 73.4 °F
DIN 53504, S2
Elongation at Break 200 %
@Temperature 23.0 °C
200 %
@Temperature 73.4 °F
DIN 53504, R1
100% Modulus 5.90 MPa
@Temperature 23.0 °C
856 psi
@Temperature 73.4 °F
DIN 53504, S2
Tear Strength 8.00 kN/m
@Temperature 23.0 °C
45.6 pli
@Temperature 73.4 °F
DIN ISO 34-1
Compression Set 21 %
@Temperature 150 °C,
Time 252000 sec
21 %
@Temperature 302 °F,
Time 70.0 hour
DIN ISO 815, B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -11.0 °C12.2 °Ftest; DIN 53545, TR
Brittleness Temperature -30.0 °C-22.0 °FDIN 53546
 
Descriptive Properties
Colorblack
Microhardness (IRHD)68DIN ISO 48 Procedure M

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFREU9091 / 293628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.