MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® LLDPE MG500026 PE (Asia)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE MG50026 is a high flow Linear Low Density Polyethylene grade with a narrow molecular weight distribution. SABIC® LLDPE MG500026 resin is in powder form and is designed to give excellent flow properties with better low temperature toughness, stress crack resistance and gloss.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/ccASTM D1505
ESCR 100% Igepal® 6.0 hourF50; Based on compression molded sheet.; ASTM D1693B
ESCR 10% Igepal® 3.0 hourF50; Based on compression molded sheet.; ASTM D1693B
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength at Break 8.00 MPaBased on injection molded specimens.; ASTM D638
Tensile Strength, Yield 10.0 MPaBased on injection molded specimens.; ASTM D638
Elongation at Break >= 350 %Based on injection molded specimens.; ASTM D638
Flexural Strength 8.00 MPaASTM D790
Flexural Modulus 200 MPaASTM D790
1% Secant Modulus 240 MPaBased on injection molded specimens.; ASTM D638
Izod Impact, Notched 500 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 88.0 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11098 / 244565

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.