MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBATER PBT A9045 black 9094 PBT+PET, 45% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: PBT/PET-Blend, 45% glass fiber reinforced, optimized surface quality, improved weld line strength and reduced tendency to warp. The KEBATER PBT A9045 black 9094 color setting meets all requirements for worldwide use in contact with foodstuffs (EU 10/2011, FDA, Mercosur, China, Japan).

Properties: dimensionally stable, good chemical resistance, Good electrical properties, good gliding properties, good aging behavior, High strength, High stiffness, High wear resistance, semi-crystalline, approved for food contact use worldwide (EU 10/2011; FDA; Mercosur; China; Japan), approved for food contact (EU and FDA)

Typical areas of application: Sports & Leisure Articles, Plug, Controls, Structural components, Fasteners, Carrier, Hardware, Connecting elements, Actuating elements, Cover, Pressure cans, Housing, Handles, industrial goods, Coffee machines, media-carrying components, Pumps and motors, Pump housing, Switch

Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Agriculture, Food processing industry, Mechanical Engineering, Medical Technology, Sanitary industry

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183-1
Moisture Absorption 0.150 %0.150 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00200 cm/cm0.00200 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.00800 cm/cm0.00800 in/inISO 294-4
Melt Flow 30.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
30.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psiISO 527-1
Elongation at Break 2.00 %2.00 %ISO 527-1
Modulus of Elasticity 16.5 GPa2390 ksiISO 527-1
Charpy Impact Unnotched 6.50 J/cm²30.9 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmContact; IEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 255 - 275 °C491 - 527 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Back Pressure <= 4.00 MPa<= 580 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO692 / 326766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.