MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCO® M4 Nickel-Aluminum Bronze, Extrusion, ≤ 25.4 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: The patented process gives AMPCO M4 mechanical properties beyond the range of commercial nickel-aluminum bronzes, comparable to beryllium copper at a lower cost and without the beryllium copper industrial hygiene requirements.

Applications: AMPCO M4 was initially developed as an aircraft specification alloy for gears in retractable landing assemblies, engine spacer bearings and other similar applications. It is rapidly growing in use where higher mechanical properties at elevated temperatures together with corrosion-resistant properties are required. Typical applications include aircraft landing gear bearings and bushings, bending dies (shoes and mandrels) for the tube bending industry, gear wheels and wear/guide plates, etc..

Key Words: AMS 4590 for extrusions
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.45 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 286HB 30
Hardness, Rockwell C 29
Tensile Strength, Ultimate 1000 MPa
Tensile Strength, Yield 793 MPa
@Strain 0.5 %
Elongation at Break 8.0 %
Reduction of Area 13 %
Modulus of Elasticity 124 GPa
Compressive Yield Strength 731 MPa0.1% Perm. Set
Compressive Strength 1324 MPa
Fatigue Strength 352 MPa
@# of Cycles 1.00e+8
Shear Strength 538 MPa
Charpy Impact 7.00 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000208 ohm-cm8.2% I.A.C.S.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.450 J/g-°C
Thermal Conductivity 42.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10.5 %
Copper, Cu 77.7 - 78.2 %As Balance
Iron, Fe 4.8 %
Manganese, Mn 1.5 %
Nickel, Ni 5.0 %
Other, total <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ampco Metal AMPCO® M4 Nickel-Aluminum Bronze, Extrusion, 25.4 - 101.6 mm.
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, 25 - 50 mm.
Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, > 50 mm.
8% Aluminum Bronze, UNS C61000

NAMPCO24 / 14978

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.