MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eagle Brass 304 Austenitic Stainless Steel, Annealed
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.

Information provided by Eagle Brass Company

Key Words: ASTM A666; UNS S30400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.285 lb/in³As Annealed
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 75.0 ksi
Tensile Strength, Yield >= 30.0 ksi0.2% Offset
Elongation at Break >= 40 %in 2 inches
Tensile Modulus 28000 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µin/in-°F
@Temperature 20.0 - 649 °C
Thermal Conductivity 113 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 18 - 20 %
Iron, Fe 66.595 - 74 %Calculated as Balance
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 10.5 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
Eagle Brass 304 Austenitic Stainless Steel, 1/2 Hardened
Eagle Brass 304 Austenitic Stainless Steel, 3/4 Hardened
Eagle Brass 304 Austenitic Stainless Steel, Full Hardened
Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened

NEAGLE519 / 147499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.