MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dyna-Purge® B Purging Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: Designed for Injection and Extrusion Blow Molding

General Description:

DYNA-PURGE B is a non-abrasive, non-chemical “engineered” thermoplastic purging compound, formulated to flow naturally through the barrel and accumulator head. A non-melting but softening thermoplastic scrubs the screw and barrel, while the carrier matrix flushes away impurities.

FEATURES & BENEFITS OF DYNA-PURGE B

  • Excellent for color changes, resin changes, preventative machine maintenance, and before manual cleaning
  • Developed for purging through the barrel and die head with a minimum clearance of .025 inch (.65 mm)
  • Effective through a wide temperature range 320°F-575°F (160°C-302°C)
  • Easy to use – no process adjustment necessary – use at the resident resin processing temperature and RPM speed
  • Non-abrasive, non-melting but softening thermoplastic, which thoroughly loosens carbonized and degraded resin, allowing it to be flushed out of the system
  • Safe, non-hazardous, with no chemicals – ingredients are FDA compliant
  • Heat stable – recommended during shutdown and start-up
  • Low “cost-per-purge” – only small quantity needed to be effective
  • No mixing required – simply use “as is”
  • Unlimited shelf life

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 302 °CInjection
 160 - 302 °CExtrusion
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Amount of Purge (Extrusion)Approx. 10 lbs per diameter inch of screwL:D dependant
Amount of Purge (Injection)Approx. 2 lbs per diameter inch of screw
Minimum Orifice (Extrusion).025in, .65mmDie
Minimum Orifice (Injection).025in, .65mmNozzle
Screen Packs or other flow restrictions (Ext.)Combination of 20, 40, 60 or 80 mesh; 100 or more, use SF or F
Screen Packs or other flow restrictions (Inj.)Must have minimum clearance of .025in (.65mm)
Types of ResinsAll

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Touchstone CFOAM® 20 Structural Carbon Foam
Touchstone CFOAM® 17 Structural Carbon Foam
Hexcel® HexWeb® CR III 5/32-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Cymat A35620SC 040SS Stabilized Aluminum Foam

PSHU29 / 67562

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.