MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Categories: Polymer; Thermoset; Phenolic

Material Notes: Description: Exclusively for mechanical applications. Impact-resistant, resistant to mechanical wear, noise-reducing, low friction. Well suited for parts where there are high mechanical load and wear. Good wear resistance in aggressive and dust-filled environments. Can be lubricated with water, oil or grease. Resistant to weather and salt water. Alternative to material containing asbestos.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 PF CC 201, DIN 7735 Hgw 2082, NF C26 150 C, BS 2572 F2/1, NEMA LI 1 C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/cc
@Temperature 23.0 °C
24h/23°C/50% RH; ISO 1183-A
Water Absorption 1.0 %ISO 62-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 80.0 MPa
@Thickness >=1.50 mm
24h/23°C/50% RH; ISO 527
Flexural Strength 115 MPa
@Thickness >=1.50 mm
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 7.00 GPa
@Thickness >=1.50 mm
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 320 MPa
@Thickness >=5.00 mm
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 40.0 MPa
@Thickness >=5.00 mm
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Thickness >=5.00 mm
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+6 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Strength 1.00 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
 5.00 kV/in
@Thickness >=3.00 mm,
Temperature 90.0 °C
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
Comparative Tracking Index 100 V
@Thickness >=3.00 mm
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
IEC 60216
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Bakelite® PF 1110 Phenolic Molding Compound
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes

PELEKT036 / 126912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.