MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical Toluene
Categories: Fluid; Solvent

Material Notes: Colorless liquid with benzene odor, Heavier than air and highly inflammable, and Not soluble to water, Readily soluble in alcohol and ether

Structure & Characteristics: C6H5CH3. Synthesized by extraction (using solvent) followed by purification of pyrolysis gasoline evolved from NCC process. Although it is a methyl-substituted benzene, the benzene ring is susceptible to electrophilic substitution due to the electron-donating methyl branch. Its 2,4,6-trinitro derivative (TNT; tri-nitro-toluene) is a well known explosive agent.

Uses: Caprolactam, TPA, Phenol, Polyurethane Explosive

CAS: 108-88-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.869 - 0.873 g/ccASTM D3505
Vapor Pressure 22.0 torr
@Temperature 20.0 °C
Vapor Density=3.14
 
Thermal PropertiesOriginal ValueComments
Melting Point -95.0 °C
Boiling Point 111 °C
Distillation Temperature 110.6 °CTotal Distillation Range
Flash Point 4.00 °C
Ignition Temperature 480 °CAutoignition
 
Descriptive Properties
Color<2Acid Wash Color, ASTM D848
 <20 Pt-CoASTM D1209
ComponentsN-AROMATICS<0.5%, ASTM D2360
 SULFUR(H2S,SO2)<1 ppm, ASTM D853
Purity>99.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuBois Thermo-Quench Oil
Aluminum 201.0-T7, Sand Cast
Aluminum 201.0-T4, Sand Cast
AISI 1050 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin

PLAY767 / 148777

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.