Product Description: Features: High flow; Suitable for injection molded products where rigidity and shorter cycle times are required. Applications: Injection molding: Caps and closures; Cosmetic and toiletry components; Household and domestic articles; Outdoor furniture Availability: Africa & Middle East; Asia Pacific, Europe, Latin America, North America Additive: Unspecified Additive Features: Fast Molding Cycle; Good Rigidity; High Flow; Homopolymer Uses: Caps; Closures; Cosmetics; Filtration Media; Household Goods; Outdoor Furnishing Forms: Pellet Processing Method: Injection MoldingInformation provided by Sasol Polymers |