MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating
Categories: Polymer; Adhesive; Thermoset

Material Notes: Multi-functional UV-CC 2004 is a single component, solvent-less conformal-coating specifically formulated for rapid room temperature cure when exposed to UV light. Thin layer coatings cure almost instantly to a depth of 7 mils.

UV-CC 2004 exhibits excellent adhesion to a variety of metals, ceramics and glass filled epoxy surfaces and is designed to meet the most demanding environmental needs of today’s PCB marketplace. This low viscosity coating can be cured by exposure to UV light and secondarily with heat for shadowed areas on densely populated circuit boards. UV-CC 2004 passes the “on-part” UL-94-V test.

Processing:

UV light cure: Bondline thickness of 7 mils; Exposure time of 5 seconds.

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Water Absorption 0.080 %
Viscosity 500 cPNominal
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Elongation at Break 10 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.50e+13 ohm-cm
Surface Resistance 3.70e+14 ohm
Dielectric Constant 3.5
@Frequency 2.00e+9 Hz
Dielectric Strength 1700 V/mil
Dissipation Factor 0.030
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 69.0 µm/m-°C
@Temperature 20.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. Specifies clear but does not quantify
 
Descriptive Properties
ColorClear Liquid
Cross Hatch Adhesion1Copper
 100%G-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESINT657 / 65541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.