MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF 2-(2-Aminoethoxy) ethanol
Categories: Fluid

Material Notes: Formula: C4H11NO2

CAS :929-06-6

Description: 2-(2-Aminoethoxy)ethanol is a colorless to yellowish liquid, with an amine-like odor. It is miscible with water in all proportions.

Synonyms: 2,2’-Aminoethoxyethanol, ADG, DGA

Applications: Intermediate used in the production of Lubrification oils, Detergents and Cooling lubricants; Also used as a Gas Scrubber absorption aid

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point -10.0 °C14.0 °F
 -10.0 °C14.0 °FFreezing Point
Boiling Point 222.6 °C432.7 °F
Flash Point 127 °C261 °F
Ignition Temperature 370 °C698 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.50 %0.50 %DIN 51 777
 
Descriptive Properties
Assay<98%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MIRANATE® B Surfactant

PBASG0853 / 132486

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.