MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
3M XLD3000 Glass Bubbles
Categories: Ceramic; Glass

Material Notes: 3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with a variety of polymers to reduce the overall thermal conductivity of the composite. These composites can be coated or incorporated into deep sea oil pipelines to improve the flow assurance properties of the system. The high strength of XLD3000 glass bubbles can withstand both the high processing pressure of polymer extrusion and the pressure of seawater in many applications. The XLD3000 glass bubbles have isostatic crush strengths of 3,000 psi with a minimum of 90% survival.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.230 g/cc
Volatiles 0.50 %
Particle Size 30 µmdiameter
pH 9.55% loading in water
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 3000 psi90% survival by volume
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.780 W/m-K
@Temperature 50.0 °C
Softening Point 600 °C
 
Descriptive Properties
Alkalinity0.4 milliequivalents/gram
AppearanceWhite, powderyunaided eye
Flotation99%density <1.0 g/cc
Packing factor60%bulk density to true particle density
ShapeHollow spheres with thin walls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M S38HS Glass Bubbles
3M iM30K Glass Bubbles
3M iM16K Glass Bubbles
3M HGS8000X Glass Bubbles
3M HGS6000 Glass Bubbles

PMM33073 / 167820

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.