MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Acetron™ AF Blend / Ertacetal™ H-TF POM-H PTFE-filled, extruded
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes: This unique thermoplastic material is used in moving parts in which low friction and long wear resistance are important. The material has a high strength, toughness, dimensional stability and good machinability, plus improved wear characteristics over unfilled POM-H.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Water Absorption at Saturation 1.00 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84.0ASTM D785
Hardness, Shore D 79.0ISO 868
Tensile Strength 55.0 MPaISO 527-1/-2 (7)
Compressive Yield Strength 26.0 MPa
@Strain 1.00 %
ISO 604 (10)
 44.0 MPa
@Strain 2.00 %
ISO 604 (10)
 77.0 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 52.0 MPaASTM D732
Charpy Impact, Notched 3.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.10
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmIEC 60243-1 (15)
 400 kV/inASTM D149
Dissipation Factor 0.0100
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM E-831 (TMA)
 105 µm/m-°C
@Temperature 23.0 - 60.0 °C
 120 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.310 W/m-K
Melting Point 347 °FASTM D3418
Maximum Service Temperature, Air 190 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 244 °FASTM D648
Minimum Service Temperature, Air -20.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Limited
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Unacceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM)
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
DuPont Mobility and Materials Delrin® 511P BK402 Acetal Homopolymer (extensive stress-strain data)
Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
Mitsubishi Chemical Advanced Materials Acetron™ / Ertacetal™ H POM-H Extruded Acetal

P1SMU834 / 130657

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.