MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Taiwan PU TPUA-142A Caprolactone, TPU Shoe Adhesive
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Key features:
  • TPU shoe material, soluble in solvent
  • Excellent initial adhesive strength
  • High bonding strength to a variety of substrate
  • Fast crystallization rate
  • Good heat resistance
Application: This series of material is suitable to be used as TPU shoe adhesive (solvent based adhesive), and used on textile Industry and others

Features: This TPU shoe material for solvent based adhesive has good adhesion to a variety of substrates - TPU, Nylon, PVC, Leather, Synthetic Leather, Polyester, Fabrics, etc.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 400 - 2400 cP15% solid content in MEK
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 9.00 - 15.0 kg(f)/cm²Initial, PVC vs. PVC After 5 mins
 
Processing PropertiesOriginal ValueComments
Cure Time >= 8.00 hourTack Time, PVC vs.PVC
 
Descriptive Properties
Crystallization ratevery slow
Max. Toluene in Solvent30-35%
Temperature55-65°CActivation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTAIWPU104 / 305834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.