MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alfa Chemistry Materials Fluorene
Material Notes: Fluorene is a white leaflets. Sublimes easily under a vacuum. Fluorescent when impure.

Solubility: Freely soluble in glacial acetic acid; soluble in hot alcohol; Slightly soluble in ethanol; soluble in ethyl ether, acetone, benzene, carbon disulfide; Soluble in carbon tetrachloride, toluene, glacial acetic acid, pyridine; very soluble in methanol

Stability: Stable under recommended storage conditions.

Molecular Formula: C13H10

IUPAC Name: 9H-fluorene

SMILES: C1C2=CC=CC=C2C3=CC=CC=C31

InChI=1S/C13H10/c1-3-7-12-10(5-1)9-11-6-2-4-8-13(11)12/h1-8H,9H2; InChiKey = NIHNNTQXNPWCJQ-UHFFFAOYSA-N

Alfa Chemistry Materials product group: Semiconductor

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.203 g/cc
@Temperature 0.000 °C
0.04346 lb/in³
@Temperature 32.0 °F
Solubility in Water 0.00 %0.00 %Insoluble
Molecular Weight 166.22 g/mol166.22 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 116 - 117 °C241 - 243 °F
Boiling Point 295 °C
@Pressure 0.101 MPa
563 °F
@Pressure 14.7 psi
Flash Point 151.0 °C303.8 °Fclosed cup
 
Descriptive Properties
CAS Number86-73-7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA69319 / 303683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.