MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen EP300K Polypropylene, Impact Modified; Molded/Extruded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP300K is a low fluidity impact copolymer suitable for injection molding applications. The product exhibits very high impact strength even at low temperature combined with a good stiffness. Moplen EP300K is typically used in a wide range of applications including house ware items and crates. Applications: Caps & Closures, Containers, House wares, Sports, Leisure & Toys.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 53.0 MPaISO 2039-1
Tensile Strength, Yield 27.0 MPaISO 527-1,-2
Elongation at Break >= 50 %ISO 527-1,-2
Elongation at Yield 9.0 %ISO 527-1,-2
Tensile Modulus 1200 MPaISO 527-1,-2
Charpy Impact, Notched 4.50 kJ/m²
@Temperature -20.0 °C
Type 1, Edgewise, Notch A; ISO 179
 5.50 kJ/m²
@Temperature 0.000 °C
Type 1, Edgewise, Notch A; ISO 179
 13.0 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 150 °CA50; ISO 306
Brittleness Temperature 0.000 °CISO 6603-2
 
Descriptive Properties
Processing MethodInjection Molding, Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene
Arkema Rilsan® BMNO TLD PA11
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Delrin Delrin® 300TE NC010 POM-I
Covestro Makrolon® 2806 Polycarbonate

PEQT8909 / 220543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.