MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraton® D1186 B (SBS) Branched Triblock Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identified:
Kraton D1186 BT - supplied as a porous pellet dusted with talc

Region: North America, Europe, Asia Pacific, Japan, and South America

Uses: Kraton D1186 B polymer is used as a modifier of bitumen in roofing felt compounds, roads and pipe coating. It may also be suitable for use in formulating adhesives, sealants and coatings and in the modification of polymers.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 2781
Bulk Density 0.400 g/ccASTM D 1895 method B
Volatiles <= 0.30 %KM 04
Viscosity 1000 - 1400 cP15% Toluene Solution at 25°C; KM 06
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Ash <= 0.50 %BT; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
@Time 10.0 sec
Typical values on polymer compression molded at 150°C; ISO 868
Tensile Strength 24.0 MPaMeasured on films cast from a solution in toluene; ISO 37
Elongation at Break 800 %measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00300 GPa
@Strain 300 %
film cast from poluene solution; ISO 37
 
Descriptive Properties
ContentAntioxidant<0.25%, KM 08
 Polystyrene29-31%, KM 03
 Total Extractables<1.4%, KM 05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D2122 DO (SBS) Compound
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer
Kraton® D1160 E (SIS) Linear Triblock Copolymer
Kraton® D1184 A (SBS) Branched Block Copolymer

PKRA9831 / 132730

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.