MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Protective Coating PC-Marine™ Epoxy Putty
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: PC-PUTTIES™ are hand moldable epoxy putty that are especially designed for emergency type repairs where time is of the essence.

Data provided by the manufacturer.

Key Words: PC Epoxy
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage <= 0.010 cm/cm<= 0.010 in/inASTM D2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75751 Week Cure; ASTM D2240
Compressive Yield Strength 83.0 MPa12000 psiASTM D695
Adhesive Bond Strength 4.80 MPa696 psiTensile Shear Strength; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+10 ohm-cm3.00e+10 ohm-cmASTM D257
Dielectric Strength 12.0 kV/mm305 kV/inASTM D149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPXP5 / 36424

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.