Tabular Alumina. Hydraulic bond. Kao-Tab 95C is a 95% alumina castable designed for casting. It maintains high strength throughout the temperature range up to 1870°C. Key features are high strength, high-use limit, good slag resistance, and high purity. Applications: - Cat cracker transfer lines where more abrasion resistance is needed
- Secondary ammonia reformer linings where low silica is desired
- Recovery boiler
- Upper furnace walls
- Recovery/cyclone boilers
- Lower furnace walls and floor
- Cyclone boilers
Information provided by Morgan Advanced Materials |