MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Vydyne 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. This product is available in natural only. It offers a well-balanced combination of engineering properties characterized by high melt point; high strength and rigidity; good toughness; soft hand and good chemical resistance.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Moisture Absorption at Equilibrium 2.5 %50% RH; ISO 62
Water Absorption at Saturation 8.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaConditioned; ISO 527-2
 50.0 MPaDry; ISO 527-2
Tensile Strength, Yield 25.0 MPaConditioned; ISO 527-2
 80.0 MPaDry; ISO 527-2
Film Elongation at Break, MD 450 %
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Film Elongation at Break, TD 500 %
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, MD 7.0 %
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, TD 6.7 %
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Elongation at Break >= 200 %Dry; ISO 527-2
 >= 200 %Conditioned; ISO 527-2
Elongation at Yield 5.0 %Dry; ISO 527-2
 30 %Conditioned; ISO 527-2
Tensile Modulus 500 MPaConditioned; ISO 527-2
 2700 MPaDry; ISO 527-2
Flexural Strength 8.00 MPaConditioned; ISO 178
 70.0 MPaDry; ISO 178
Flexural Modulus 250 MPaConditioned; ISO 178
 2200 MPaDry; ISO 178
Poissons Ratio 0.40Dry; ISO 527-2
Secant Modulus, MD 0.392 GPa
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Secant Modulus, TD 0.444 GPa
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 180
 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 180
 8.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 180
 NB
@Temperature 23.0 °C
Conditioned; ISO 180
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
Elmendorf Tear Strength MD 100 g
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D1922
Elmendorf Tear Strength TD 110 g
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D1922
Dart Drop Test >= 2100 g
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D1709A
Film Tensile Strength at Break, MD 121 MPa
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Break, TD 105 MPa
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-2
Melting Point 220 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 5.00 - 20.0 °CBlow Film Air Temperature
 230 - 275 °CCylinder - Extrusion
Die Temperature 240 °CExtrusion
Melt Temperature 220 °CExtrusion
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
 
Descriptive Properties
Agency RatingsEU 10/2011
 EU 2023/2006
FeaturesGood Chemical Resistance
 Good Toughness
 Heat Stabilized
 High Melt Stability
 High Rigidity
 High Strength
Melt Pressure MPa3 to 17
Screw DesignGP or Barrier
UsesFilm
 Industrial Applications
 Monofilaments
 Profiles
 Rods
 Sheet
 Tubing
 Vacuum Bagging Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® B 230 PA66/6, Conditioned
AdvanSix Aegis® HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer
Arkema Orgalloy® EM 067 HSP PA6
Ascend Performance Materials Vydyne® 00XFS Nylon 66/6 Compounding Grade
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66

PZASCE9768 / 220871

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.