MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Avient Nymax™ GF 1200 A 30 FR Natural Nylon 66 with Glass Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Molded Test Bars: Dry as Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cmASTM D955
Ash 35 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 183 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Yield 2.0 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 241 MPaASTM D790
Flexural Modulus 8960 MPaASTM D790
Izod Impact, Notched 85.4 J/m
@Thickness 1.57 mm,
Temperature -40.0 °C
Across Flow, Compression Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
@Thickness 1.57 mm
Annealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.57 mm
All colors; Internal Method
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityNorth America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
Plastcom SLOVAMID 6 NG GF 30 Polyamide 6, 30% Glass Fiber
Global Atron 602 GF-33 Natural Industrial Nylon 6, 33% Glass Filled
Evonik Vestamid® Terra DS 18-GF-30 natural color 30% Glass Filled Nylon 1010
EPICHEM PA 6/66 GF 30 Polyamide 6/66, 30% Glass

PH1PN9305 / 103141

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.