MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: PPS-GF/MD 65

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.94 g/ccISO 1183
Water Absorption 0.020 %similar to ISO 62 test
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaISO 527-1
Elongation at Break 0.80 %ISO 527-1
Tensile Modulus 19000 MPaISO 527-1
Charpy Impact Unnotched 20.0 kJ/m²ISO 179-1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°CISO 11359-1/-2
Melting Point 285 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 265 °CISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.800 mm
UL Registered; IEC 60695-11-10
 
Descriptive Properties
Resin TypePPS-GF/MD 65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Fortron® 6165 A4 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber
Avient Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
MOCOM (ALBIS) Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only)
MOCOM (ALBIS) Tedur® L 9523 PPS, 60% Glass Fiber/Mineral

PBARLO905 / 149923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.