MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow SARAN WRAP™ 3 Plastic Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic

Material Notes: SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls, in widths up to 65 inches.

Dow has sold the Saran Wrap product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 8.70 g/m²/day
@Temperature 37.8 °C
90% RH; Permatran W
Oxygen Transmission 1.20 cc-mil/100 in²-24hr-atm10% RH; ASTM D3985
Nitrogen Transmission 0.180 cc-mil/100 in²-24hr-atm10% RH; ASTM D1434
Carbon Dioxide Transmission 5.40 cc-mil/100 in²-24hr-atm10% RH; ASTM D1434
Thickness 0.500 milASTM D374
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 90 %ASTM D882
Film Elongation at Break, TD 60 %ASTM D882
Secant Modulus, MD 0.4826 GPa2% Secant; ASTM D882
Secant Modulus, TD 0.5516 GPa2% Secant; ASTM D882
Film Tensile Strength at Break, MD 13000 psiASTM D882
Film Tensile Strength at Break, TD 15000 psiASTM D882
Heat Seal Strength Initiation Temperature 141 °C0.28 lb/in heat seal strength; SWTM-19
 157 °C0.40 lb/in heat seal strength; SWTM-19
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 15 %
@Temperature 100 °C
Unrestrained, in Air
Shrinkage, TD 9.0 %
@Temperature 100 °C
Unrestrained, in Air
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ASTM D1003
Gloss 112 %45°; ASTM D2457
Transmission, Visible 86 %Clarity; ASTM D1746
 
Descriptive Properties
Air Transmission cc-mil/100 in²-24hr-atm0.3610% RH
Block Force g12SWTM-23
Cling g8SWTM-23
Yield in2/lb34600ASTM D2103

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyvinyl Dichloride (PVDC)
Dow SARAN WRAP™ 18 Plastic Film
SK Chemicals Saran® 506 Polymer
SK Chemicals Saran® 540 Vapor Retarder Film
SK Chemicals Saran® 168

PDOW1408 / 30626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.