MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Geon® Performance Solutions L6105 natural Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 818115 sec; ASTM D2240
Tensile Strength, Yield 54.8 MPa7950 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 4.72 GPa685 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 95.1 MPa13800 psiASTM D790
Flexural Modulus 4.54 GPa658 ksiASTM D790
Izod Impact, Notched 0.430 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.806 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy  53.4 J/cm
@Temperature 23.0 °C
0.100 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
 53.4 J/cm
@Temperature 23.0 °C
0.100 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 46.0 µm/m-°C25.6 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C
@Treatment Temp. 60.0 °C
174 °F
@Treatment Temp. 140 °F
Annealed; ASTM D648
 77.2 °C
@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
171 °F
@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Treatment Temp. 60.0 °C
171 °F
@Treatment Temp. 140 °F
Annealed; ASTM D648
 73.9 °C
@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
165 °F
@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 - 3.00 mm
V-0
@Thickness 0.0591 - 0.118 in
natural; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
FeaturesHigh Stiffness
 Low CLTE
FormsCube
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification12474ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 81510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80530 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 83510 Polyvinyl Chloride, Rigid
Overview of materials for PVC, Rigid Grade
Overview of materials for PVC, Sheet Grade

PH0POL1067 / 145636

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.