Notes: Medalist® MD-12342 is a high performance thermoplastic elastomer specifically designed for healthcare and medical applications. It is a low density, low hardness, RoHS compliant grade that can be sterilized and is suitable for both injection molding extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Ethylene Oxide Sterilizable; Excellent Processability; Good Colorability; Good Flexibility; Good Moldability; Good Processability; High Elasticity; High Purity; Kink Resistant; Low Density; Low Hardness; No Animal Derived Component; Radiation (Gamma) Resistant Uses: Medical Devices; Medical Packaging; Medical/Healthcare Applications; Pharmaceutical Packaging; Pharmaceuticals; Transparent or Translucent Parts; Tubing Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex |