MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

General Plastics LAST-A-FOAM® FR-7140 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Feature:
  • Will not warp or bow
  • Chemically inert
  • Dimensionally stable
  • Grain-free stock material
  • Fine-cell structures
  • Closed-cell
  • Easily bonded and finished with a wide variety of adhesives and coatings
  • Low densities can be hand carved and shaped easily with common woodworking tools
  • Higher densities are available for CNC work where more accuracy is desired
  • Custom sizes available
Applications:
  • Proof stock
  • Composite core
  • Prototype models
  • Styling models
  • Tooling aids
  • Check fixtures
  • Mold patterns
  • Foundry patterns
  • Decorative trim

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.641 g/cc0.0232 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 76.676.6cut foam surface; ASTM D2240
Tensile Strength 15.98 MPa2317 psiParallel to Rise; ASTM D1623
 17.06 MPa2475 psiPerpendicular to Rise; ASTM D1623
Flexural Strength 23.36 MPa3388 psiRise Parallel to Test Span; ASTM D790
 24.25 MPa3517 psiRise Parallel to Beam Thick.; ASTM D790
Flexural Modulus 0.89804 GPa130.25 ksiRise Parallel to Beam Thick.; ASTM D790
 0.898049 GPa130.251 ksiRise Parallel to Test Span; ASTM D790
Compressive Strength  14.71 MPa
@Temperature 93.3 °C
2134 psi
@Temperature 200 °F
Parallel to Rise; ASTM D1621
 15.11 MPa
@Temperature 93.3 °C
2191 psi
@Temperature 200 °F
Perpendicular to Rise; ASTM D1621
 29.1 MPa
@Temperature 23.9 °C
4220 psi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 29.39 MPa
@Temperature 23.9 °C
4263 psi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
Compressive Modulus  0.35724 GPa
@Temperature 93.3 °C
51.814 ksi
@Temperature 200 °F
Perpendicular to Rise; ASTM D1621
 0.37939 GPa
@Temperature 93.3 °C
55.026 ksi
@Temperature 200 °F
Parallel to Rise; ASTM D1621
 0.78400 GPa
@Temperature 23.9 °C
113.71 ksi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 0.801005 GPa
@Temperature 23.9 °C
116.176 ksi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
Poissons Ratio 0.300.30
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C
@Temperature -45.6 - 93.3 °C
31.0 µin/in-°F
@Temperature -50.0 - 200 °F
GP Method
Thermal Conductivity 0.0918 W/m-K0.637 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 119 °C246 °FASTM E1824
 
Descriptive Properties
Tumbling Friability (%)0.120 mins at 60 rpm, ASTM C421
Water Absorption0.004 lbs/ft²ASTM D2842

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-6725 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-7120 Polyurethane Foam
Sawbones Solid Rigid Polyurethane Foam 15 pcf Density
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Lord Adhesives Chemglaze® V175 Polyurethane Coating

PGENR057 / 186843

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.