MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S21904 (Alloy 21-6-9) Stainless Steel, sheet and strip 0% cold reduction, stress relieved at 480°C (900°F) for 1 hour
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Austenitic, high strength, excellent corrosion resistance, and low magnetic permeability. Applications include aircraft applications such as ducting and bellows systems, tail pipes and exhaust systems, clamps, fasteners, flanges, and hydraulic tubing.

Key Words: UNS S21904, AMS 5595, AMS 5656, ASME SA412, ASTM A269 (XM-11), ASTM A276 (XM-11), ASTM A314 (XM-11), ASTM A412 (XM-11), ASTM A473 (XM-11), ASTM A580 (XM-11)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 162162Converted from Rockwell B hardness.
Hardness, Rockwell B 9494
Hardness, Vickers 213213Converted from Rockwell B hardness.
Tensile Strength, Ultimate 803 MPa116000 psi
Tensile Strength, Yield 494 MPa
@Strain 0.2 %
71600 psi
@Strain 0.2 %
Elongation at Break 44 %44 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Machinability 30 %30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000730 ohm-cm0.0000730 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.7 µm/m-°C
@Temperature 25.0 - 95.0 °C
9.28 µin/in-°F
@Temperature 77.0 - 203 °F
 17.3 µm/m-°C
@Temperature 25.0 - 205 °C
9.61 µin/in-°F
@Temperature 77.0 - 401 °F
Annealed
 18.2 µm/m-°C
@Temperature 25.0 - 315 °C
10.1 µin/in-°F
@Temperature 77.0 - 599 °F
Annealed
 19.1 µm/m-°C
@Temperature 25.0 - 540 °C
10.6 µin/in-°F
@Temperature 77.0 - 1000 °F
 20.0 µm/m-°C
@Temperature 25.0 - 760 °C
11.1 µin/in-°F
@Temperature 77.0 - 1400 °F
Annealed
 20.0 µm/m-°C
@Temperature 25.0 - 870 °C
11.1 µin/in-°F
@Temperature 77.0 - 1600 °F
Annealed
 20.5 µm/m-°C
@Temperature 25.0 - 980 °C
11.4 µin/in-°F
@Temperature 77.0 - 1800 °F
Annealed
Specific Heat Capacity 0.480 J/g-°C0.115 BTU/lb-°FTypical value for stainless steel.
Thermal Conductivity  7.80 W/m-K
@Temperature -180 °C
54.1 BTU-in/hr-ft²-°F
@Temperature -292 °F
 10.9 W/m-K
@Temperature -73.0 °C
75.6 BTU-in/hr-ft²-°F
@Temperature -99.4 °F
 13.8 W/m-K
@Temperature 95.0 °C
95.8 BTU-in/hr-ft²-°F
@Temperature 203 °F
 16.1 W/m-K
@Temperature 205 °C
112 BTU-in/hr-ft²-°F
@Temperature 401 °F
 18.2 W/m-K
@Temperature 315 °C
126 BTU-in/hr-ft²-°F
@Temperature 599 °F
 20.2 W/m-K
@Temperature 425 °C
140 BTU-in/hr-ft²-°F
@Temperature 797 °F
 22.5 W/m-K
@Temperature 540 °C
156 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 24.7 W/m-K
@Temperature 650 °C
171 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 26.8 W/m-K
@Temperature 760 °C
186 BTU-in/hr-ft²-°F
@Temperature 1400 °F
 28.9 W/m-K
@Temperature 870 °C
201 BTU-in/hr-ft²-°F
@Temperature 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.040 %<= 0.040 %
Chromium, Cr 20 %20 %
Iron, Fe 64 %64 %
Manganese, Mn 9.0 %9.0 %
Nickel, Ni 6.0 %6.0 %
Nitrogen, N 0.23 %0.23 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
414 Stainless Steel, tempered at 508°C
AISI Type S21800 Stainless Steel, 10% cold reduction
AISI Type S21800 Stainless Steel, 20% cold reduction
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 60% cold reduction
AISI Type 430F(Se) Stainless Steel annealed bar

MQM22EL / 13736

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.