SBR–1500 is a high molecular weight styrene butadiene rubber combining good extrusion behavior and superior compound properties. SBR 1500 contains antioxidant to avoid product degradation. The high strength and great toughness of rubber permit the use of its elastic qualities. The properties of rubber show excellent resistance to cutting, tearing and abrasion. It has a relatively long, useful life under a wide variety of conduction. Applications: tires, tread rubber, molded and extruded mechanical goods. Information provided by Iran Petrochemical Commercial Co. |