MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Dow SE 4445 CV KIT
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.36 g/cc
@Temperature 25.0 °C
Viscosity 14000 cPdynamic
 
Mechanical PropertiesOriginal ValueComments
Penetration P(60), 1/10 mm 57
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+15 ohm-cm
Dielectric Constant 6.0
@Frequency 1e+6 Hz
Dielectric Strength 127 V/mil
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.26 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -45.0 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 45.0 min
@Temperature 125 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Colorgrey
Hydrophobicyes
Self Levelingyes
Water Resistantyes
Working Time (min)300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Jet-melt™ 3748 V-O Light Yellow Adhesive: High-Melt Technology
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets
Tra-Con Tra-Cast 9182A Semi-Rigid Flame Retardant Epoxy Encapsulant
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray

PDOWCO349 / 106050

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.