MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Solvay DAPCO™ 3012 Self-Extinguishing, Low Density Honeycomb Filler
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DAPCO™ 3012 is a two-component, self-extinguishing epoxy filler.

Features & Benefits:

  • Flowable
  • Cures at room temperature
  • Excellent adhesion to metal, composites, fiberglass, Kydex™
  • Very low water absorption
  • Good chemical resistance, especially to aircraft fluids
  • Can be threaded, countersunk, drilled, cut, etc. without cracking or chipping
  • 100% solids
  • Side-by-side applicator capacity
Applications: DAPCO 3012 is commonly used for potting/stiffening and edge filling in honeycomb core. It is also used for bonding Kydex™, Kevlar™, fiberglass and metal to each other and insert installation.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.801 g/cc
Solids Content 100 %Part A
 100 %Part B
 100 %Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
Tensile Strength 1775 psi
Flexural Modulus 200000 psi
Compressive Strength 4000 psi
Adhesive Bond Strength 1800 psiShear, Aluminum (2024-T3) at 150°F (66°C)
 2200 psiShear, Aluminum (2024-T3) at room temperature
Peel Strength 6.00 pliT-Peel
 12.0 pliBell
 
Descriptive Properties
ColorLight yellowMixed
 WhitePart A
 YellowPart B
Mix Ratio1:1Volume
 100:75Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Solvay DAPCO™ 3021C Low Viscosity, Self-Extinguishing Honeycomb Filler
Celanese Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Solvay DAPCO™ 3050 Epoxy Potting Compound
Solvay DAPCO™ 3004 Rapid Cure Epoxy Adhesive & Repair Compound

PCYTED017 / 180319

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.