MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unitika AXF-1500-05 Conditioned
Categories: Polymer; Thermoplastic; Polyarylate

Material Notes: Characteristics:
  • Lubricant grade of AX1500, excellent in heat and chemical resistances

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPaASTM D638
Elongation at Break 22 %ASTM D638
Flexural Strength 78.0 MPaASTM D790
Flexural Modulus 1100 MPaASTM D790
Izod Impact, Notched 147 J/m
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Constant 3.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 635 V/milASTM D149
Dissipation Factor 0.040
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 80 secASTM D495
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 230 °C
Middle Barrel Temperature 240 - 260 °C
Front Barrel Temperature 250 - 270 °C
Nozzle Temperature 250 - 270 °C
Mold Temperature 70.0 - 90.0 °Cactual surface temp
Drying Temperature 100 °C
Dry Time 10.0 - 24.0 hour
Back Pressure 0.490 - 1.47 MPagage pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitika AXG-1500-300 Conditioned
Unitika PT-3020
Unitika LM-8503-10
Unitika FUN-8000
Unitika C300VN

PUNITIK896 / 177916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.