MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® VTR-8500 is a peroxide cured polymer intended to be an upgrade to Viton® GLT. VTR-8500 utilizes an Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to GLT and GLT 305
  • Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
  • Shows excellent physical properties with high elongation in either the original or aging tests
  • Shows similar to improved heat, fluids, and low temperature resistance compared to GLT
  • Shows excellent compression set resistance with little (2 hr at 232°C ) or no postcure

It is recommended if mixing in an internal mixer to use at least a 70% load factor. The recommended process aid for VTR-8500 is 0.5 phr of Armeen® 18D.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Tensile Strength, Ultimate 17.6 MPaCured 7 min at 177°C and Post Cured 16 hr at 232°C
Tensile Strength, Yield 0.000600 GPa10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Elongation at Break 181 %Cured 7 min at 177°C and Post Cured 16 hr at 232°C
100% Modulus 0.00590 GPa
@Strain 100 %
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Compression Set 16 %
@Temperature 200 °C
Method B, O-rings 22 hr at 200°C (Cured 7 min at 177°C and Post Cured 16 hr at 232°C)
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -30.6 °CTR-10
Glass Transition Temp, Tg -30.7 °CDSC
 
Descriptive Properties
Formulation as Tested100Viton® VTR-8500
 3Zinc Oxide
 3Diak™ 7
 3Luperox® 101-XL
 30N990 Carbon Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials VTR 8550 (GFLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation
Chemours Viton® F-605C Fluoroelastomer (FKM)
430 Stainless Steel annealed bar
DuPont Mobility and Materials VTR 8650 (GBL-S) Peroxide Cured Fluoroelastomer (FKM) Formulation
Daikin DAI-EL® G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content

PDVDA43 / 34012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.