System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Super Asia Polyblend WT1210 TPE
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
Material Notes:
Stationery, toy, hand tool handle, bicycle accessories
Information provided by Super Asia Polyblend Co., Ltd
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.970
-
1.03
g/cc
0.0350
-
0.0372
lb/in³
ASTM D792
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
7.0 - 13
7.0 - 13
ASTM D2240
Tensile Strength
1.96
MPa
284
psi
ASTM D412
1.47
MPa
@Temperature 136 °C,
Time 605000 sec
213
psi
@Temperature 277 °F,
Time 168 hour
High Temperature Aging; ASTM D573
1.57
MPa
@Temperature 63.0 °C,
Time 1.80e+6 sec
228
psi
@Temperature 145 °F,
Time 500 hour
Heat Resistance; W-O-M
Elongation at Break
850 %
850 %
ASTM D412
680 %
@Temperature 136 °C,
Time 605000 sec
680 %
@Temperature 277 °F,
Time 168 hour
High Temperature Aging; ASTM D573
722.5 %
@Temperature 63.0 °C,
Time 1.80e+6 sec
722.5 %
@Temperature 145 °F,
Time 500 hour
Heat Resistance; W-O-M
Rebound
70 %
70 %
Elasticity; CNS K1392
Tear Strength Test
3.0
3.0
[kg/cm2], ASTM D624 Die C
Thermal Properties
Metric
English
Comments
Brittleness Temperature
-60.0
°C
-76.0
°F
ASTM D746
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSUPER018 / 305683
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.