MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Versalis KOSTIL B266 Styrene Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Symbol according to ISO 1043-1: SAN

Grade designation according to ISO 4894-SAN 2,M,105-15

Standard injection moulding grade with good chemical resistance Application fields:

  • household and small appliances
  • large appliances (internal parts)
  • lighting
  • cosmetics, medical and pharmaceutical items
  • bathroom furnishing
  • others (catering, stationery, toys, displays)

Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains release agent.

ISO data.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: SAN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Melt Flow 18 g/10 min
@Load 10.0 kg,
Temperature 220 °C
18 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 67.0 MPa9720 psi5 mm/min
Elongation at Break 2.5 %2.5 %5 mm/min
Tensile Modulus 3.55 GPa515 ksi1 mm/min
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²
 1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °F
Vicat Softening Point 105 °C221 °F50°C/hr; 50N
Glass Transition Temp, Tg 103 °C217 °F10°C/min test
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Manufacturer specifies 'transparent' but doesn't quantify.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unipetrol PE HD LITEN® MB/ML 71 HDPE
Trinseo CALIBRE™ 201-22 Polycarbonate Resin
INEOS Styrolution Terlux® 2802 Transparent MABS
INEOS Styrolution Luran® 378P Crystal Clear Transparent SAN
Evonik Trogamid® T5000 Nylon 6-3

PENJ41 / 35917

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.