MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT ALPA-LSR 160201 Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a 2-part addition cure silicone elastomer system for Liquid Injection Molding (LSR). After mixing parts ‘A’ and ‘B’ in the correct proportions, the system will cure at elevated temperatures, usually in the range of 100 °C to 180 °C. The cycle time depends mainly on the temperature and the shape of the mould. The cured rubber exhibits excellent physical and electrical properties.

Key Features

  • Product is suitable for Liquid Injection Molding process
  • Curing speed can be accelerated by temperature
  • Very good mechanical properties
  • Easy demoulding

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³A; DIN 53 479
 1.13 g/cc0.0408 lb/in³B; DIN 53 479
 1.13 g/cc0.0408 lb/in³Cured; DIN 53 479
Brookfield Viscosity 600 cP600 cPA
 600 cP600 cPB
 600 cP600 cPMixed
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060DIN 53 505
Tensile Strength 10.0 MPa1450 psiDIN 53 504, S 3 A
Elongation at Break 400 %400 %DIN 53 504, S 3 A
Tear Strength 30.3 kN/m173 pliASTM D 624, Die B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time >= 2880 min>= 48.0 hourDe-mould Time / Full Cure
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColortranslucentA
 translucentB
 translucentCured Product
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL162 / 314645

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.