MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Applications: thick films and lasers

Key Words: Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.75 g/cc0.135 lb/in³ASTM-C373
Water Absorption 0.00 %0.00 %ASTM-C373
Particle Size 1.5 µm1.5 µmGrain Size; Intercept Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 45 N 8282ASTM-E18
Modulus of Elasticity 331 GPa48000 ksiASTM-C623
Flexural Strength 482 MPa69900 psiASTM-F394
Poissons Ratio 0.250.25ASTM-C623
Shear Modulus 132 GPa19100 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 4.00e+14 ohm-cm>= 4.00e+14 ohm-cmASTM-D1829
Dielectric Constant 9.55
@Frequency 1e+6 Hz
9.55
@Frequency 1e+6 Hz
ASTM-D150
Dielectric Strength 18.5 kV/mm
@Thickness 1.02 mm
470 kV/in
@Thickness 0.0400 in
60 cycles AC avg. RMS; ASTM-D149
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
ASTM-D150
Dielectric Loss Index  0.0040
@Frequency 1e+6 Hz
0.0040
@Frequency 1e+6 Hz
Loss Factor; ASTM-D150
 0.0090
@Frequency 1000 Hz
0.0090
@Frequency 1000 Hz
Loss Factor; ASTM-D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.40 µm/m-°C
@Temperature 25.0 - 200 °C
3.56 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM-C372
 7.20 µm/m-°C
@Temperature 25.0 - 500 °C
4.00 µin/in-°F
@Temperature 77.0 - 932 °F
ASTM-C372
 7.90 µm/m-°C
@Temperature 25.0 - 800 °C
4.39 µin/in-°F
@Temperature 77.0 - 1470 °F
ASTM-C372
 8.20 µm/m-°C
@Temperature 25.0 - 1000 °C
4.56 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM-C372
Thermal Conductivity  12.0 W/m-K
@Temperature 400 °C
83.3 BTU-in/hr-ft²-°F
@Temperature 752 °F
 20.0 W/m-K
@Temperature 100 °C
139 BTU-in/hr-ft²-°F
@Temperature 212 °F
 26.0 W/m-K
@Temperature 20.0 °C
180 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 96 %96 %
 
Descriptive Properties
ColorWhite
PermeabilityNIL
Surface Finish - (µin.)<0.89as-fired; Profilometer, 0.0002" Radius Stylus, 0.100" Cutoff, ANSI/ASME B46.1
 <35CLA; Profilometer, 0.0002" Radius Stylus, 0.100" Cutoff, ANSI/ASME B46.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4)
Ceradyne Ceralloy® 1370DP Aluminum Nitride
Ceradyne Ceralloy® 1370CS Aluminum Nitride
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4)

CCOOR932 / 104636

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.