MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).

Applications

TX is used for:

  • flat display substrates
  • optical components
  • miscellaneous goods.
TP/TH are used for:
  • food package sheeting as well as in manufacturing
  • electronic equipment and components
  • miscellaneous goods
TE/CL are for:
  • electronic equipment and components
  • information equipment components
  • AV equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.127 g/ccISO 1183
Melt Flow 1.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 87ISO 2039-2
Flexural Strength 120 MPaISO 178
Flexural Modulus 3.35 GPa2mm/min; ISO 178
Charpy Impact, Notched 0.200 J/cm²ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CISO 75-2
Vicat Softening Point 101 °C50N; ISO 306
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Haze 0.20 %
@Thickness 2.00 mm
ISO 14782
Transmission, Visible 92 %
@Thickness 2.00 mm
ISO 13468-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Network Polymers MS 300 Styrene Methyl Methacrylate Copolymer
Chi Mei Acryrex® CM-211 PMMA
Overview of materials for Polypropylene Copolymer
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade
American Polymers API 392 Polystyrene

PDENK012 / 29676

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.