MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increased chromium, an aluminum content which together provide outstanding resistance to oxidation. In addition, AL 601 alloy has good resistant to environments containing carbon and sulfur and this alloy resists aqueous corrosion. The AL 601 alloy is used in aerospace applications, for heat and chemical processing equipment, and in power generation, pollution control and heat treating applications. Forming, machining and welding properties are similar to those of stable austenitic stainless steels.

Information provided by Allegheny Ludlum

Key Words: DIN 2.4851; ASTM B-168; AMS 5870
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.05 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80Typical
Tensile Strength, Ultimate 790 MPaTypical
Tensile Strength, Yield 440 MPaTypical
Elongation at Break 45 %typical in 2"
Reduction of Area 60 %Typical
Modulus of Elasticity 205 GPa
Charpy Impact 150 JTypical
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 27.0 °C
 14.6 µm/m-°C
@Temperature 20.0 - 315 °C
 15.3 µm/m-°C
@Temperature 20.0 - 538 °C
 18.3 µm/m-°C
@Temperature 20.0 - 1093 °C
Specific Heat Capacity 0.460 J/g-°C
Maximum Service Temperature, Air 1093 °CHigh oxidation resistance due to tenacious oxide film formation.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.35 %
Carbon, C 0.050 %
Chromium, Cr 23 %
Copper, Cu 0.25 %
Iron, Fe 14.1 %
Manganese, Mn 0.50 %
Nickel, Ni 60.5 %
Silicon, Si 0.25 %
Sulfur, S 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600
Special Metals INCONEL® Alloy 601
Special Metals INCOLOY® Alloy 825
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Carlson C 800H Nickel-Iron-Chromium Alloy

NLN60A / 18018

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.