MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 1137 Epoxy Microballoon Repair Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 1137 is a sag resistant syntactic-foam formulation developed for aerospace honeycomb, fillet, edge-fill, contour repair, bonding, potting and casting applications where a light-weight, low shrinkage and low expansion material is required. This adhesive is easily mixed and handled at room temperature, and it develops strong, highly reliable bonds to most surfaces -- including metals, glass and glass fabrics, and many plastics. TRA-BOND 1137 is a completely unicellular material composed of micron-sized phenolic spheres in a high-performance epoxy binder, has a very uniform point-to-point structure and exhibits low shrinkage during cure, good dimensional stability, low density, high strength-to-weight ratio, high dielectric strength, and a low dielectric constant. The fully cured adhesive is a strong, light weight and durable electrical insulator which can be cut, drilled sawed and shaped (as needed) with ordinary shop tools. In addition, TRA-BOND 1137 is resistant to water, weather, gases and vapors, salt and salt solutions, mild acids and alkalis, alcohol, jet fuels, gasoline and other petroleum products, and many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.650 g/ccMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 25 min
 
Descriptive Properties
Color Red-Brown
Mix Ratio, parts by weight100/18Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Stanyl® TW341 PA46, Conditioned, Heat Stabilized

PTRAC000 / 70928

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.