MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Aremco’s high temperature ceramic adhesives are formulated using a broad range of ceramics fillers and inorganic binders, and are ideal for bonding, potting and sealing ceramics, composites, graphite, refractory metals, quartz, and semiconductors for applications to 3200°F (1760°C).

Typical Applications:
Electrical

  • Halogen Lamps
  • Heaters
  • Igniters
  • Fiberoptics
  • Resistors
  • Solid Oxide Fuel Cells
Instruments & Sensors
  • Gas Chromatographs
  • High Vacuum Components
  • Liquid Metal Inclusion Counters
  • Mass Spectrometers
  • Oxygen Analyzers
  • Strain Gauges
  • Semiconductors
  • Temperature Probes
Mechanical
  • Ceramic Honeycombs
  • Ceramic Textiles
  • Graphite Blocks
  • Refractory Insulation
  • Sagger Plates
  • Thread-Locking

Vendors: Aremco’s ceramic and graphite adhesives are ideal for bonding, potting and sealing probes, sensors, halogen lamps, igniters, power resistors, cartridge heaters, filters, fiberoptics, honeycombs, and graphite structures to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.80 - 1.95 g/cc
Volatile Organic Compounds (VOC) Content 0.00 g/l
Viscosity 2500 - 5000 cP
 
Mechanical PropertiesOriginal ValueComments
Impact Test 60.0 ft-lbTorque Strength; curing at 1000°F
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 142 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.30 µin/in-°F
Maximum Service Temperature, Air 3000 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °CApplication Temp
Cure Time 2.00 hour
@Temperature 93.3 °C
preceded by 1-4 hour air set
Shelf Life 6.00 Month
@Temperature 4.44 - 32.2 °C
 
Descriptive Properties
Acid ResistanceGoodafter curing at 700°F for 2 hours
Alkali ResistanceGoodafter curing at 700°F for 2 hours
ColorWhite
Moisture ResistanceExcellentafter curing at 700°F for 2 hours
SolventWater
Thinner670-T

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone

CAREM17a / 138291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.