MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® TSGL-50-4 nat PA666-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 40% Glass Fiber Reinforced

Material Notes: Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following key-properties:
  • high stiffness and strength even after conditioning and over a wide temperature range
  • excellent notched impact resistance also at low temperatures
  • low creep
  • high heat distortion temperatures
  • good dimensional stability and little warpage
  • good surface appearance and ease of processing
The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement. Grilon TSGL-50/4 natural is used in the following market segments:
  • automotive
  • mechanical engineering
  • household and appliances
The glass-fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccDry; ISO 1183
Water Absorption 4.5 %Sim. to ISO 62
Moisture Absorption 1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 200 MPaConditioned; ISO 2039-1
 310 MPaDry; ISO 2039-1
Tensile Strength at Break 185 MPaConditioned; ISO 527-1/-2
 265 MPaDry; ISO 527-1/-2
Elongation at Break 2.3 %Dry; ISO 527-1/-2
 2.6 %Conditioned; ISO 527-1/-2
Tensile Modulus 12500 MPaConditioned; ISO 527-1/-2
 17400 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 105 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 40.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 40.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 45.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 45.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+11 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 22.0 kV/mmConditioned; IEC 60243-1
 27.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°CISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 120 - 130 °CLong Term; ISO 2578
 220 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 230 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Exterior
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesLong Fiber Reinforced
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Stanyl® TW271F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America)
Envalior Stanyl® TW200F6 PA46-GF30, Dry, 30% Glass Filled, Heat Stabilized
EMS-Grivory Grilon® TSG-50/4 PA666-GF50
EMS-Grivory Grilon® TSG-35/4 H black 9836 PA666-GF35
EMS-Grivory Grilon® TSG-30/4 LF 15 PA666-(GF+Z)45

PGRH285 / 156994

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.