Product Description: 45 Shore A TPE (Styrenic Block Copolymer based) available in black and natural for injection molding and extrusion applications. This grade offers excellent resiliency and elasticity. Availability: North America Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Colorability; Good Processability; High Elasticity; High Heat Resistance; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Resilient; Solvent Resistant; UV Resistant Appearance: Black; Natural Color Processing Method: Extrusion; Injection Molding Information provided by Entec Polymers |