Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
KaMin Polyfil® XB Kaolin Clay - Waterwashed
Categories:
Ceramic
;
Clay
;
Kaolin Clay
Material Notes:
Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.
Industry:
Rubber & Plastic
Uses:
Non-Black Rubber, General Rubber Goods, EPDM, Wire & Cable
Information provided by KaMin LLC.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
2.60
g/cc
2.60
g/cc
Bulk Density
0.577
-
0.705
g/cc
0.0208
-
0.0255
lb/in³
Loose
Solids Content
69.5 - 71 %
69.5 - 71 %
Slurry
Brightness
86 - 87.5 %
86 - 87.5 %
Reflectance (TAPPI)
Oil Absorption
42 %
42 %
Fineness
>= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium
<= 1.5 %
<= 1.5 %
As Produced
Particle Size
0.50
µm
0.50
µm
Average Stokes Equivalent Diameter
2.3
µm
2.3
µm
Median (Malvern Laser)
Particle Mesh Size
325
Mesh
325
Mesh
0.005% Retained
pH
6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area
17
m²/g
17
m²/g
BET
Brookfield Viscosity
450
cP
@Temperature 25.0 °C
450
cP
@Temperature 77.0 °F
20 RPM
Descriptive Properties
Bulking Value
21.7 lb.gal
CAS Number
1332-58-7
Crystalline Silica (quartz)
<0.1%
Physical Forms
Dry, Slurry
Shipping Point
Macon, GA
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
CKAMAN948 / 178419
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.