MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem LH 0820/30 AF LLDPE Blown Film Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1

Applications: Lamination; heavy duty bags; blends with LDPE and HDPE; valvulated heavy duty bags.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D1505
Thickness 38.0 microns
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 947 %ASTM D882
Film Elongation at Break, TD 1185 %ASTM D882
Secant Modulus, MD 0.174 GPa1%; ASTM D882
Secant Modulus, TD 0.184 GPa1%; ASTM D882
Coefficient of Friction 0.67ASTM D1894
Elmendorf Tear Strength, MD 11.0 g/micronASTM 1922
Elmendorf Tear Strength, TD 20.0 g/micronASTM 1922
Dart Drop 4.55 g/micronASTM D1709
Film Tensile Strength at Break, MD 47.0 MPaASTM D882
Film Tensile Strength at Break, TD 37.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 34.8 %ASTM D1003
Gloss 4.9 %60° angle; ASTM D2457
 
Descriptive Properties
AdditivesAntiblock and PPA
Minimum Recommended Thickness50 µm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer
Braskem EB 853/72 LDPE Blown Film Extrusion Polyethylene

PBRAS098 / 27832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.