MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) Altech® NXT PP PP-H A 2040/456.01 LE GF40 CP 40% Glass Filled PP Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Polypropylene Homopolymer. 40% glass fibers. Chemically coupled, low emission (VDA 278), low emission (VDA 277), low emission (VDA 270), low emission (DIN 75201-B), high heat stabilized, high stiffness, high toughness. Application: automotive, various

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm
@Time 86400 sec
ISO 294-4
Spiral Flow 29.0 cm
@Thickness 1.00 mm
 60.0 cm
@Thickness 2.00 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527-1/-2
Elongation at Yield 2.5 %ISO 527-1/-2
Tensile Modulus 9400 MPaISO 527-1/-2
Flexural Strength 150 MPaISO 178
Flexural Modulus 8250 MPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
 40.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 8.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 154 °CISO 75-1/-2
Vicat Softening Point 143 °CB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 270 °Cinjection molding
Mold Temperature 20.0 - 90.0 °Cinjection molding
Drying Temperature 80.0 °C
@Time 7200 - 10800 sec
for superior surface quality, and for better emission properties

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) Altech® NXT PP PP-B A 2035/450 GF35 CP 35% Glass Filled PP Copolymer
E-Polymers SEPAZ® LH30 PP Homopolymer LFT Resin
Entec Hypro™ F PPC-GF40 Natural Impact Polypropylene, 40% Glass Reinforced
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)
Celanese Celstran® PP-GF40-04 natural PP, 40% Glass Reinforced

PALBIS9917 / 221013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.