MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PSM Industries Ferro-TiC® PK Maraging Steel
Categories: Ceramic; Carbide; Metal; Ferrous Metal; Maraging Steel

Material Notes: Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.

Combination of excellent transverse rupture strength, impact strength, and corrosion resistance. Good thermal shock resistance. Magnetic.

    Ferro-TiC® Unique Characteristics
  • Provides the lightweight, size, stability, and hardness
  • Virtually porosity free - significantly better than the A1 ASTM B-276-79 Standard
  • Low specific mass. Ferro-Tic® is 10-20% lighter than its steel counterpart and about 50% lighter than tungsten carbide
  • 10 times the wear resistance of tool steels
  • Economical fabrication (conventionally machinable in the annealed stage by milling and turning, conventionally heat treatable to achieve high hardness)
  • 50-90% less linear size change in heat treat than tool steels

Information Provided by Ferro-TiC®, a division of PSM Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 50Annealed
 61Hardened
Flexural Strength 200000 psiTransverse Rupture
Compressive Strength 417 ksi
Charpy Impact Unnotched 35.08 ft-lb/in²
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.11 µin/in-°F
@Temperature 21.1 - 449 °C
Maximum Service Temperature, Air 840 °F
 
Descriptive Properties
Carbide (Vol. %)42
Linear Size Change Thru Heat Treat %-0.029
Thermal Shock (No. Cycles)84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EOS MS1 Maraging Steel Sintered on EOSINT M 270
PSM Industries Ferro-TiC® MS-5A Age Hardenable Martensitic Stainless Steel
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 32 mm
AISI Grade 18Ni (350) Maraging Steel nominal annealed properties

NPSM023 / 93214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.