MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Matexcel NAT-1510 Chitin Nanogel
Categories: Wood and Natural Products

Material Notes: Chitin nanogel has rich functional groups, can be redispersed after drying, and has good biological safety and compatibility. It has broad application prospects in agriculture, medicine, food, beauty and health care, sensors and other fields.

NAT-1510; Chitin Nanogel

Morphology: Powder

Key Words: Synonyms: Chitin Nanogel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 20.0 °C
 
Descriptive Properties
Product overviewThe product can be provided in wet or dry (re-dispersible) formulations according to needs. The product has the functions of natural antibacterial, weight loss and lipid lowering. The product can form functional 3D materials including films, gels, silk threads, etc., and can also be flexibly compounded with a variety of substrates to provide nano-enhancement effects.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1960 / 300591

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.